From: Elemental sulfur coarsening kinetics

Figure 4

Dynamic light scattering results illustrating effect of SDS surfactant on S 8(Weimarn) particle coarsening kinetics at 3 temperatures. Solid circles represent S8(Weimarn) sols without SDS while hollow circles represent S8(Weimarn) formed in the presence of SDS. Blue symbols are at 25°C, green symbols at 50°C, and red symbols at 75°C.